What the Lab Found in Our Car Mats

The solvent-free protein leather of the Eco-Leather base layer passed EN 71-3, the European toy-safety test for heavy metals. Formaldehyde and the 24 restricted aromatic amines were not detected. Tested by Sharp Standard Testing Technology (SST), Dongguan, report SST26002338 of 18 July 2026.

The results

Four tests, one sample

TestMethodResult
Heavy metals (toy safety) EN 71-3:2019+A2:2024, Annex E, Category III Passed. Lead and mercury below 2.5 mg/kg (limits 23 and 94 mg/kg). Aluminium, antimony, tin and zinc were found in traces, all far inside their limits.
Formaldehyde ISO 14184-1:2011 Not detected (limit of detection 16 mg/kg).
24 restricted aromatic amines (released by some azo dyes) With reference to ISO 14362-1/-3 and ISO 17234-1/-2 None detected (limit of detection 5 mg/kg each).
Abrasion (Martindale, dry) ISO 12947-2:2016 No wear from 20,000 up to 100,000 cycles. The report sets no pass mark.

What it covers

Read it for what it is

  • A test report, not a certificate. A laboratory tested a sample and reported what it found. There is no certificate or accreditation mark, so we say "tested", never "certified".
  • One sample of the base-layer leather. The material supplier sent the lab one sample of the solvent-free protein leather. The results apply to that sample. The Tex-Mesh top layer is a separate material and was not tested.
  • "Not detected" means below the lab's limit of detection, not zero. That is why we never write "0%" or "100% free".
  • EN 71-3 is about heavy metals only. Formaldehyde and the aromatic amines are separate tests, listed above.
  • Not tested: smell, heat, waterproofing, grip, or anything about children or pets. We make no claim about those from this report.

Why these tests

What each one looks for

  • Heavy metals. EN 71-3 measures how much lead, mercury and 17 other elements can migrate out of a material. It is the test used for children's toys in Europe.
  • Formaldehyde. Used in some resins and finishes on leathers and textiles.
  • Aromatic amines. Some azo dyes can break down into these; 24 of them are restricted for materials in contact with skin.
  • Abrasion. The Martindale test rubs the surface for thousands of cycles to see when it wears. It speaks to scuffing from shoes, not to cuts or punctures.

Same build in every pattern

Every EZYMAT set has the same Eco-Leather base and Tex-Mesh top layer; only the stitching changes.